There are wet flowers (water vapor) on the surface of the fireproof board, and the edge is serious

2022-09-23 16:19:21
a

There are wet flowers (water vapor) on the surface of the fireproof board, and the edge is serious

Causes:

1. The content of volatiles is too high after drying the impregnated paper

2. The solvent used for printing wood grain ink or dye is inappropriate

3. Moisture absorption (moisture regain) of adhesive film paper after soaking and drying

Solution:

1. Reduce the content of volatile matter after drying the impregnated paper

2. Change the solvent for ink (dye)

3. Pay attention to the storage of adhesive film paper, which can generally be covered with plastic cloth

Fireproof board, fire-resistant board, fireproof board manufacturer

The surface of the fire-proof plate and the surface of the decorative plate are cracked

Causes:

1. The resin reaction is too tender and the molecule is too small

2. Incomplete curing of resin

3. The glue content of the surface film paper is too high

Solution:

1. Stop using unqualified resin

2. Appropriately increase the hot pressing temperature or extend the hot pressing time

3. Control the glue content of the surface film paper